Improved recovery of a lowgrade refractory gold ore using
Jul 01 2014 · In this work different flotation–preoxidation–cyanidation methods are considered for treating a lowgrade refractory gold ore On the one hand the results of selective flotation show that 22 and 311 of total Sb and As respectively remained in the final tailings and only about 28 of the total Au remained for further cyanidation processes